3D printing SLASLSFDM

SLA, SLS or FDM: picking a 3D printing process for functional prototypes

All three make a part in a day. They do not make the same part. A comparison of resolution, tolerance, anisotropy and cost per cubic centimetre — with the applications each process actually suits.

6 min read
Clear SLA printed prototype housing next to a grey primed version of the same part

The three processes are often quoted interchangeably because they share a lead time. They differ in almost everything else, and choosing badly usually shows up later as a part that splits along a layer line or a fit that drifts by 0.3 mm.

The comparison that matters

 SLA (resin)SLS (nylon)FDM (filament)
Typical tolerance±0.1 mm or 0.2% ±0.3 mm or 0.3%±0.5 mm or 0.5%
Layer thickness0.05–0.1 mm0.1–0.12 mm0.1–0.3 mm
SurfaceSmooth, paintableFine sandy grainVisible layer lines
StrengthBrittle, not for snap fitsTough, near-isotropicStrong in XY, weak in Z
Min wall0.6 mm0.8–1.0 mm1.2–2.0 mm
Cost driverVolume + supportBuild volume (nesting)Volume + support + time
Best forVisual models, clear parts, fine detailFunctional parts, living hinges, ductsJigs, fixtures, large brackets

Swipe sideways to see all columns →

SLA: when appearance and detail decide

Resin printing wins on surface finish and small features — 0.4 mm text, 0.6 mm walls, sharp edges. Clear and translucent resins make light pipes and lenses; grey resin takes paint and looks like a production part in a photo. The limitation is mechanical: standard resins are brittle, so snap fits and press fits crack. Use tough or ABS-like resins if the part has to flex, and expect them to still be less ductile than SLS nylon.

SLS: when the part has to work

Sintered PA12 is the default for functional prototypes. It is tough, fatigue-resistant and nearly isotropic, because the powder bed supports the part so there are no layer-direction weak points. Living hinges, snap clips, cable guides and ducting all behave like the moulded part. The trade-off is surface: a fine grain that cannot be polished to gloss, and a tolerance that drifts on large thin features. Glass-filled PA12 (PA12-GF) adds stiffness and heat resistance at the cost of a rougher finish.

FDM: when size or cost decides

Fused filament is the cheapest way to make something large, and the only practical option for a 400 mm bracket. It is also the process where orientation matters most: a part loaded across the layer lines will delaminate. Design for it — put the load in-plane, thicken walls to 2 mm and above, and avoid fine detail. For jigs, fixtures, drill guides and shop-floor tooling it is often the correct answer, not a compromise.

A decision rule that works

  1. Does it have to look like the final part? Yes → SLA, then paint.
  2. Does it have to survive repeated assembly? Yes → SLS PA12.
  3. Is it larger than 300 mm, or does it need to be cheap? Yes → FDM.
  4. Does it need to be watertight or airtight? SLS, or SLA with a thickened wall — FDM will leak at the seams.
  5. Is it a mould master for vacuum casting? SLA, at 0.05 mm layers, polished.
Print what you are testing. If the prototype is for a photo shoot, buy surface. If it is for a drop test, buy toughness. Paying for both in one process usually means paying twice.

Finishing changes the equation

Bead blasting smooths SLS to a uniform matte. Primer and paint make SLA look moulded. Vapour smoothing gives ABS-like FDM parts a near-injection finish but softens detail. Each adds a day and 15–40% to the price, and each is worth it only if the part will be photographed or handled by a customer.

We run all three in house, so the quote compares processes rather than defending one. Send the model and tell us what the part has to survive.

Keep reading

Related articles

Your programme

Put this article to work on a real part

Send a STEP file, a drawing and a quantity curve. You will get a price, a lead time and a DFM note within 12 working hours.